Description
Suspension of dextran coated iron oxide nanoparticles for MRI angiography, high resolution cell tracking, magnetic particle imaging, and MRI liver imaging following intravascular injection
Properties
- Core particle size: 6 nm ± 2nm
- Z-Average (DLS): 155 nm nm
- Z-Potential: -1.76 (+/- 1.0) mV
- Concentration: 10 mg per ml
- Particles/ml: ∼1E+15